MCC110 and selenium
Has anyone experienced discolouration of the paper base when selenium toning this paper. I would descibe it as a overall light straw colour. The prints were processed in Agfa ne, stop bath and two bath fix in Hypam followed by an hour in a Nova slot washer. The selenium toner is Fotospeed, perhaps a bit strong at 1+12. All chemicals were mixed freshly. My intention was to briefly selenium (60-90secs) followed after a thorough wash by partial weak sepia for the hilights. I can only think I had the selenium a tad to warm. This kind of stain has not happened previously with any other paper I have used with this routine and it is has been my established working method for sel/sepia toning for a number of years.
|
#2
|
||||
|
||||
Sorry to hear of your problem
My only suggestion would be a Hypo Clearing Agent pre-toning bath. Tim Rudman in his Toning Booking mentions light discolouration of the paper base if the paper is not sufficiently alkali prior to the Se bath Martin |
#3
|
||||
|
||||
Thank you Martin. I'll try HCA and re read Tim's book. Strange it has only happened with MCC.
|
#4
|
||||
|
||||
Not I. I do selenium tone it, in Kodak RST 1+19, typically for 3-4 minutes. Much longer and I get too much eggplant cast for my tastes. But I do wash aid and long soak before toning.
|
#5
|
||||
|
||||
Quote:
HCA may not be the answer to your problem - but its an easy one to eliminate. I don't actually use manufactured HCA but a Teaspoon full of Sodium Sulphite per 1L of water and then pour it away at the end of the Toning Session Sodium Sulphite is the main active ingredient in HCA I get mine from Silverprint and a small container lasts me well over a year Good luck Martin |
#6
|
||||
|
||||
Thank you again Martin. I have some Sodium Sulphite, I'll try that and various dilution and temps of selenium this weekend.
|
#7
|
|||
|
|||
T tone MC110 in 1:19 KRST for a few minutes without any problems -certainly no change in base colour.
|
Support our Sponsors, they keep FADU free: AG Photographic The Imaging Warehouse Process Supplies RH Designs Second-hand Darkroom Supplies |
Thread Tools | Search this Thread |
Display Modes | |
|
|
Similar Threads | ||||
Thread | Thread Starter | Forum | Replies | Last Post |
Problem with selenium toning | Miha | Monochrome printing techniques | 24 | 4th June 2011 09:50 PM |
Selenium Toner Disposal | Neil Smith | Toning | 25 | 30th November 2010 04:55 PM |
Moersch selenium vs Ilford vs Kodak | Jacques | Toning | 4 | 1st March 2010 02:46 PM |
Selenium Toning | hugh | Monochrome printing techniques | 15 | 29th August 2009 08:33 AM |
Source of Powdered Selenium | Pete O | Chemical formulae | 8 | 16th August 2009 08:21 PM |