Non-allergenic, environmentally friendly print developer.
I'm always on the look out for recipes with a low(er) impact on the environment and this caught my attention. It's E72, which gives similar results to D72 (sold by Kodak as Dektol). It doesn't contain Hydroquinone (not good for aquatic life or sewerage systems apparently), or metol - a known cause of dermatitis.
Water (50DegC ish) 750ml Phenidone 0.5g Sodium Sulphite (anh) 45g Ascorbic Acid* 19g Sodium Carbonate 90g Cold water to 1l *Ascorbic acid is available from health food shops as Vitamin C powder - my wife used it in breadmaking, so I didn't even have to buy any! Dilute 1:2 for use (it will work up to 1:4 but with lower contrast) I was initally a bit sceptical, but after a trial today I am pleasantly surprised. It's quite fast, and gives a good neutral-cool tone on Ilford MG FB. I've yet to try it with warm-tone papers. Rob |
#2
|
|||
|
|||
Quote:
|
#3
|
||||
|
||||
Quote:
Steve. |
#4
|
|||
|
|||
As well as the Eco D76 variant being talked about just now, this is another formula that I will try as well.
Thanks Rob. Terry S |
#5
|
||||
|
||||
I've been using this as my standard neutral-tone print developer for some years now. It does work well with warm tone paper diluted at 1:4 although full development will take up to 5 minutes depending on temperature. For warmer tones add 10ml of 10% potassium bromide solution per litre (more than that gives warmer tones but slows down developing dramatically).
|
#6
|
|||
|
|||
I've just reread this, and as my print developer is nearly finished, I think I'll give it a go before ordering some more of my usual.
Has anyone else tried this and want to comment? Terry S |
#7
|
|||
|
|||
Just remember that "Vitamin C Powder" can be ascorbic acid, or sodium ascorbate, both useful in developers but you need to be aware of the difference. There is also calcium ascorbate at my local pharmacy, and you don't want calcium in your developer.
Also, in the original post, should there be some bromide? Last edited by Stocky; 8th November 2023 at 09:27 PM. |
#8
|
|||
|
|||
And don't forget that that I have started a new post about ascorbic acid / vitamin C type developers, initially focusing on E72, as a HQ free print developer, with the post being started in October 2023:
http://www.film-and-darkroom-user.or...ad.php?t=14758 Terry S |
Support our Sponsors, they keep FADU free: AG Photographic The Imaging Warehouse Process Supplies RH Designs Second-hand Darkroom Supplies |
Thread Tools | Search this Thread |
Display Modes | |
|
|
Similar Threads | ||||
Thread | Thread Starter | Forum | Replies | Last Post |
D-23 Film Developer | Barry | Chemical formulae | 18 | 25th September 2012 01:10 AM |
Print Developer Temperature ? | vincent | Monochrome printing techniques | 6 | 1st March 2009 10:52 AM |
D 163 Print Developer | Dave miller | Chemical formulae | 3 | 18th February 2009 10:11 AM |
WS-print developer-volume | Trevor Crone | Monochrome printing techniques | 37 | 29th November 2008 05:08 PM |
Which Film Developer? | Barry | Chemical formulae | 31 | 23rd November 2008 05:11 PM |